Corning Launches 2.0 High-index Glass For AR

Apr 25, 2026

Back in January 2026, Corning released a new high-index glass with a refractive index of 2.0. It's designed for AR and MR headsets, supporting wider fields of view and sharper image quality. The glass comes in 150–300mm wafer formats, and it helps make those headsets thinner and lighter – something the whole industry has been pushing for.