• 16

    Jun, 2026

    The core technology of cover glass

    The cover glass, it's technology lies in balancing hardness(scratch resistance), toughness(drop resistance) and optical clarity but remain cost effective for mass production. 1.Material & processe

  • 15

    Jun, 2026

    How to use screen print on glass

    In a piece of complete cover glass, you may wondering how the black borders, heating lines or logo to be located such precise. It's about the screen, imagine it looks like a super fine stencil. What's

  • 13

    Jun, 2026

    How to solve color difference?

    In sourcing glass with silkscreen print, customers often face problem about color difference from each batch or even single batch especially white color, why for that? Below are the reasons to cause i

  • 13

    Jun, 2026

    What's the difference between low temperature ink and high temperature ink?

    When you need to customize silkscreen print glass, you may asked about which kind of ink should be printed, low temperature or high temperature inks. So below comparisons can tell you difference among

  • 13

    Jun, 2026

    Do you know how to test if the glass can resist impact?

    In normal life, the normal glass may break easily under hit by stone. But tempering can improve the impact resistance 5-6 times. Do you know if the impact resistance ability can meet your expect? IK t

  • 13

    Jun, 2026

    How to test if the glass fully tempered?

    In daily application, fully tempered glass has 5-6 times hardness than regular glass. But by visual, we couldn't identify whether tempered or not(of course there's a way to use polarizing film by expe

  • 13

    Jun, 2026

    Cover glass mechanical and reloiability test

    The test are cover glass proves its actual toughness. Most of them are destructive or designed to mimic longterm use. Surface stress: It measures both the depth of compressive stress layer and the ove

  • 12

    Jun, 2026

    How to verify AR coating durability in glass processing

    1.What we can do: Environmental stress test Damp heat(85/85): 2000 hours in 85°C and 85% RH(relative humidity), verify when transmittance loss below 1%. Xenon arc weathering: Full spectrum sunlight si

  • 11

    Jun, 2026

    Global Cover Glass: What's Happening Right Now

    The cover glass market is doing about $9.8 billion in 2026, growing roughly 9% a year. But the real story isn't the number - it's what's changing inside the glass itself. The Big Shift: Fr

  • 10

    Jun, 2026

    What's the update news about AF glass?

    1.The market is heating up The super hydrophobic display glass market jumped from 1.53 billion USD(2025) to 1.84 billion(2026), which is 20.3% growth. It's expect 3.82 billion USD in 2030. Drivers

  • 10

    Jun, 2026

    How to make a test for glass AR coating?

    1.What's the meaning and purpose AR coating(means anti reflective coating, which apply in glass surface to improve light transmittance), the test purpose is to evaluate optical performance, mechan

  • 10

    Jun, 2026

    Guide to AG glass

    What's AG glass mean? AG(anti glare) glass has a textured surface that scatters light instead of reflecting. Result? The screens stay readable under bright sunlight or harsh indoor lighting. 3 way